Titanas jūrų įrangai

Mar 02, 2022

Titanium alloy can not only make marine equipment develop towards "deep, large, far, high ", but also fully realize the same life as the main body of marine equipment. It is the best choice for marine equipment. At present, China pays more attention to the application of titanium in marine equipment, and the amount of titanium used is also increasing. Deep-sea pressure shell, seawater pipeline, cylinder superstructure, frame, etc. will become the key development direction of marine titanium.

marine equipment

Šiuo metu laivybos pramonėje namuose ir užsienyje yra daug titano pritaikymų.

However, the material system in relevant specifications is not perfect. It is hoped that relevant units will organize discussion and improve the material system in current relevant codes such as Titanium Pressure Vessel, Material and Welding, so as to facilitate the designer's reference.

Upper buildings: 

Šiuo metu yra keletas pritaikymo pavyzdžių vidaus karo laivų antstatams, pvz., Ti70 (TA23) stiebui, TA5 ir TA7 strypai radaro antenai, TA2 ir TA5 plokštės angaro dangai ir rėmo konstrukcijai.

Titanas taip pat plačiai naudojamas viršutinėse LPD17 amfibinio doko transporto laivo pastatų srityse, sumažinant jo masę apie 50 procentų ir labai pagerinant jo stabilumą.

Gamybos pritaikymas kitose srityse

Be didelio titano kiekio, naudojamo aukščiau minėtame slėgiui{0}}atspariame korpuse, vamzdynų sistemoje ir antstatuose, kiti komponentai taip pat naudingi laivų įrangoje namuose ir užsienyje.