Nikelio rūšys ir cheminė sudėtis
| Gryno nikelio klasė | Ni+Co | Cu | Si | Mn | C | Mg | S | Fe | Iš viso priemaišų | UNS žymėjimas |
| nemažiau nei | ||||||||||
| N2 | 99.98 | 0.001 | 0.003 | .002 | .005 | .003 | .001 | .007 | .02 | |
| N4 | 99.9 | 0.015 | 0.03 | .002 | .01 | .01 | .001 | .04 | 0.1 | N02201 |
| N6 | 99.5 | 0.06 | 0.10 | .05 | .10 | .10 | .005 | .10 | 0.5 | N02200 |
| N8 | 99.0 | 0.15 | 0.15 | .20 | .20 | .10 | .015 | .30 | 1.0 | |
| DN | 99.35 | 0.06 | 0.02-0.10 | 0.05 | .02.10 | .02-.10 | .005 | .10 | 0.35 | |
| NY1 | 99.7 | 0.1 | 0.1 | - | .02 | .10 | .005 | .10 | 0.3 | |
| NY2 | 99.4 | 0.01-0.10 | 0.1 | - | - | - | 0.002-0.01 | .10 | 0.6 | |
| NY3 | 99.0 | 0.15 | 0.2 | - | 0.1 | 10 | 0.005 | .25 | 1.0 | |
| NMg0,1 | 99.6 | 0.05 | 0.02 | .05 | .05 | 0.07~0.15 | 0.005 | .07 | .40 | |
| NSI0.19 | 99.4 | 0.05 | 0.15~0.25 | .05 | .10 | .05 | 0.005 | .07 | .50 | |
Nikelio atsparumas korozijai
Nikelis yra ypač atsparus šarminei korozijai ir yra gana stabilus aukštoje temperatūroje arba liepsnoje ištirpusiame šarme, todėl daugiausia naudojamas šarmų pramonėje. Normalioje temperatūroje sraigė yra itin stabili jūros vandenyje, druskos tirpale ir organinėje terpėje (pvz., riebalų rūgštis, fenolis, fermentacija ir kt.), neatspari neorganinės rūgšties korozijai, taip pat stabili acto rūgštyje ir šviesioje rūgštyje.